Siccator crystallinus infrarubrus ad pelliculas PET fabricandas


Proiectum est ad fabricandas pelliculas supellectilis PET.
Tota incepta undecim unitates IRD requirunt.
IRD pro PET Masterbatch 6 unitates 150kg/h/unitas.

>> Materbatch PET siccare et crystallizare uno gradu per XX minutas
>> Humiditas finalis est ≤50ppm
>> Nulla materia effluens, viscosa vel cohaerens
>> Facile purgandum
IRD pro APET Particle 700kg/h 1 unitas et 300kg/h 1 unitas

Siccatio et crystallizatio uno gradu
>>Umiditas initialis ≤3000ppm
>>Temperatura siccationis 160℃
>>Tempus siccandi 20 minuta
>> Humiditas finalis 50ppm
IRD pro SK PETG 300kg/h 1 unitas et 80kg/h 1 unitas

>>Umiditas initialis ≤780ppm
>>Temperatura siccationis 105℃
>>Tempus siccandi 20 minuta
>> Humiditas finalis 50ppm
IRD Pro Granulis rPET 1 unitas

Tempus publicationis: VII Aprilis MMXXIII